Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Latrobe 14-4CrMo Stainless Tool Steel

Category Metal , Ferrous Metal , Martensitic , Stainless Steel , Tool Steel
Manufacturer Latrobe Steel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe 14-4CrMo Stainless Tool Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
14-4CrMo is a wear resistant, martensitic stainless tool steel that exhibits better corrosion resistance than Type 440C stainless steel. The molybdenum in the steel provides superior corrosion resistance compared to some higher-chromium stainless steels. The combination of the high carbon and molybdenum contents results in the formation of hard, wear-resistant molybdenum carbides in the microstructure of the steel. These molybdenum carbides provide superior wear resistance and edge retention for cutting tools and knives. Typical applications include knife blades, bearings, valve components, and bushings.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.78 g/cc
7.78 g/cc
Density 7.78 g/cc
0.281 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 60
60
Oil Quenched from 1010°C, 45 minutes
60.5
60.5
Oil Quenched from 1010°C with cryogenic treatment at -73°C, 45 minutes
62.5
62.5
Oil Quenched from 1080°C, 45 minutes
63.3
63.3
Oil Quenched from 1038°C, 45 minutes
63.5
63.5
Oil Quenched from 1038°C with cryogenic treatment at -73°C, 45 minutes
65
65
Oil Quenched from 1080°C with cryogenic treatment at -73°C, 45 minutes
Modulus of Elasticity 207 GPa
30000 ksi
Machinability 60 - 65 %
60 - 65 %
1% Carbon Steel
Thermal Properties Metric English Comments
CTE, linear 10.3 µm/m-°C

@Temperature 20.0 - 100 °C
5.72 µin/in-°F

@Temperature 68.0 - 212 °F
10.8 µm/m-°C

@Temperature 20.0 - 316 °C
6.00 µin/in-°F

@Temperature 68.0 - 601 °F
Thermal Conductivity 24.2 W/m-K

@Temperature 392 °C
168 BTU-in/hr-ft²-°F

@Temperature 738 °F
Component Elements Properties Metric English Comments
Carbon, C 1.05 %
1.05 %
Chromium, Cr 14 %
14 %
Iron, Fe 80.15 %
80.15 %
Manganese, Mn 0.50 %
0.50 %
Molybdenum, Mo 4.0 %
4.0 %
Silicon, Si 0.30 %
0.30 %
Users viewing this material also viewed the following: