Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical 25SPR GPPS

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Molded, Unreinforced
Manufacturer LG Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical 25SPR GPPS.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superior extrusion processing suitable for OPS, PSP and synthetic wood, Applications include food receptacles, stationery, audio tapes, toys, PSP sheet, and film
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 2.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 51.1 MPa
7410 psi
50 mm/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
50 mm/min; ASTM D638
Flexural Yield Strength 103.1 MPa
14950 psi
15 mm/min; ASTM D790
Flexural Modulus 3.10 GPa
450 ksi
15 mm/min; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C

@Thickness 12.7 mm
189 °F

@Thickness 0.500 in
Unannealed; ASTM D648
Vicat Softening Point 105 °C
221 °F
1000 g; ASTM D1525
Flammability, UL94 HB
HB
1/16 in
HB
HB
1/8 in
Flame Spread 26.0 mm/min

@Thickness 3.17 mm
1.02 in/min

@Thickness 0.125 in
FH3