Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kennametal Stellite Stellite® 31 PM with P/M Processing; heat treated at 93°C (200°F) and water quenched

Category Metal , Nonferrous Metal , Cobalt Alloy , Superalloy
Manufacturer Kennametal Stellite
Trade Name Stellite®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Kennametal Stellite Stellite® 31 PM with P/M Processing; heat treated at 93°C (200°F) and water quenched.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Typical applications include, miscellaneous wear parts. Data provided by the manufacturer, Deloro Stellite Inc.Product of former Deloro Stellite Inc.
Physical Properties Metric English Comments
Density 8.45 g/cc
0.305 lb/in³
P/M (98%)
8.61 g/cc
0.311 lb/in³
Theoretical
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 828 MPa
120000 psi
414 MPa
<br>@Temperature 760 °C
60000 psi
<br>@Temperature 1400 °F
614 MPa
<br>@Temperature 649 °C
89100 psi
<br>@Temperature 1200 °F
676 MPa
<br>@Temperature 538 °C
98000 psi
<br>@Temperature 1000 °F
Tensile Strength, Yield 497 MPa
<br>@Strain 0.200 %
72100 psi
<br>@Strain 0.200 %
290 MPa
<br>@Strain 0.200 %,<br> Temperature 649 °C
42100 psi
<br>@Strain 0.200 %,<br> Temperature 1200 °F
311 MPa
<br>@Strain 0.200 %,<br> Temperature 760 °C
45100 psi
<br>@Strain 0.200 %,<br> Temperature 1400 °F
331 MPa
<br>@Strain 0.200 %,<br> Temperature 538 °C
48000 psi
<br>@Strain 0.200 %,<br> Temperature 1000 °F
Elongation at Break 4.0 %
4.0 %
in 25.4 mm
13 %
<br>@Temperature 649 °C
13 %
<br>@Temperature 1200 °F
in 25.4 mm
14 %
<br>@Temperature 538 °C
14 %
<br>@Temperature 1000 °F
in 25.4 mm
21 %
<br>@Temperature 760 °C
21 %
<br>@Temperature 1400 °F
in 25.4 mm
Thermal Properties Metric English Comments
CTE, linear 14.1 µm/m-°C
<br>@Temperature 21.0 - 316 °C
7.83 µin/in-°F
<br>@Temperature 69.8 - 601 °F
14.5 µm/m-°C
<br>@Temperature 21.0 - 427 °C
8.06 µin/in-°F
<br>@Temperature 69.8 - 801 °F
15.1 µm/m-°C
<br>@Temperature 21.0 - 538 °C
8.39 µin/in-°F
<br>@Temperature 69.8 - 1000 °F
15.7 µm/m-°C
<br>@Temperature 21.1 - 649 °C
8.72 µin/in-°F
<br>@Temperature 70.0 - 1200 °F
16.5 µm/m-°C
<br>@Temperature 21.1 - 816 °C
9.17 µin/in-°F
<br>@Temperature 70.0 - 1500 °F
16.6 µm/m-°C
<br>@Temperature 21.1 - 871 °C
9.22 µin/in-°F
<br>@Temperature 70.0 - 1600 °F
Component Elements Properties Metric English Comments
Carbon, C 0.50 %
0.50 %
Chromium, Cr 25.5 %
25.5 %
Cobalt, Co 50 %
50 %
As remainder
Iron, Fe <= 2.0 %
<= 2.0 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Nickel, Ni 10.5 %
10.5 %
Other <= 2.0 %
<= 2.0 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.040 %
<= 0.040 %
Tungsten, W 7.5 %
7.5 %