Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Karina 55/200 Clear PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 55/200 Clear PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.18 - 1.24 g/cc
1.18 - 1.24 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 53 - 57

@Time 15.0 sec
53 - 57

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
Tear Strength >= 25.0 kN/m
>= 143 pli
DIN 53507
Abrasion <= 300
<= 300
mm<sup>3</sup>; DIN 53516
Descriptive Properties Value Comments
Application Sandals