Polymer Property : Tear Strength = 25.0 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 25.0 kN/m
143 pli
D624
Polykemi AB POLYelast TPE Z506 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
Tear Strength 25.0 kN/m
143 pli
D624
Polykemi AB POLYelast TPE Z600A Thermoplastic Elastomer, SEBS-based, Co-injection Grade
Information provided by Polykemi AB
Tear Strength >= 25.0 kN/m
>= 143 pli
DIN 53507
Karina E CAK 60-48/1 Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tear Strength >= 25.0 kN/m
>= 143 pli
DIN 53507
Karina E CAK 65/48/1-CS Black PVC Compound
Reclaimed PVC Compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tear Strength 25.0 kN/m
143 pli
Die B
Momentive Performance Materials Siloprenâ„¢ LSR 2540 Liquid Silicone Rubber - Textile Coating
This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
Tear Strength 25.0 kN/m
143 pli
Die B
Momentive Performance Materials Silplusâ„¢ 50 MP Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 25.0 kN/m
143 pli
Die B
Momentive Performance Materials TSE 2297 Heat Cured Rubber - High Duro Translucent
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 25.0 - 35.0 kN/m
143 - 200 pli
NF EN ISO 1421
Isoflon Tisoflon® 15S1 SILICONE ONE SIDE Silicone Coated Glass Fabric
Silicone coated Glass fabric TISOFLON®Information provided by Isoflon.
Tear Strength 25.0 kN/m
143 pli
Die B
Momentive Performance Materials Addisilâ„¢ 2080 E Industrial Extrusion Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 25.0 kN/m
143 pli
ISO 6383
SABIC Innovative Plastics NORYL WCA105 PPE-TPE (Asia Pacific)
Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requir..
Tear Strength 25.0 kN/m
143 pli
ISO 6383
SABIC Innovative Plastics NORYL WCA105 PPE-TPE (Europe-Africa-Middle East)
Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requir..
Tear Strength 25.0 - 30.0 kN/m
143 - 171 pli
Die B; ASTM 624
Wacker Silicones Geniomer® 140 Silicone TPE
SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas..
Tear Strength 25.0 kN/m
143 pli
Trelleborg R350 Natural Rubber Polyisoprene
All information provided by Trelleborg
Tear Strength 25.0 kN/m
143 pli
Trelleborg R490 Commercial Natural Rubber Polyisoprene
All information provided by Trelleborg
Tear Strength 25.0 kN/m
143 pli
Trelleborg R583 Commercial Natural Rubber Polyisoprene
All information provided by Trelleborg
Tear Strength 25.0 kN/m
143 pli
GB/T 529
Chengdu Polyster 4502 High Performance Grade TPV
Excellent resiliency, good hand feel, paintable.Information provided by Chengdu Polyster Co., Ltd.
Tear Strength 25.0 kN/m
143 pli
ASTM D624
ELASTO UK Dryflex® 660650S SEBS Based Material, Semi-Filled Qualities, 65A Hardness, Natural
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
Tear Strength 25.0 kN/m
143 pli
ASTM D624
ELASTO UK Dryflex® 662650S SEBS Based Material, Semi-Filled Qualities, 65A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
Tear Strength 25.0 kN/m
143 pli
Trelleborg B636 Nitrile Rubber
Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi..
Tear Strength >= 25.0 kN/m
>= 143 pli
DIN 53507
Karina E 60/200 Cristal Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.