Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Permabond QFS10 Cyanoacrylate Activator

Category Other Engineering Material , Catalyst/Initiator
Manufacturer Permabond
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond QFS10 Cyanoacrylate Activator.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The PERMABOND QFS 10 accelerates the cure of cyanoacrylate adhesives to provide a shorter set time. It can be used in a variety of applications but is especially useful when bonding porous or poorly mated parts. PERMABOND QFS10 cures the adhesive before it soaks into a porous surface or runs out from between parts with sizable gaps. It can be used to accelerate cure on sensitive plastic surfaces such as polycarbonate without causing stress cracking. No discoloration of the part surface is observed when using PERMABOND QFS 10. The activator can be sprayed on the surface of the cyanoacrylate to accelerate curing in wire tacking or similar bonding applications. PERMABOND QFS 10 contains a specially chosen initiator in a non-halogenated solvent that is not ozone depleting. This solvent evaporates quickly to leave a thin film of the initiator on the surface to be bonded. Features & Benefits: Contains no ozone depleting agent Rapid setting on closely mated parts Faster cure through gaps Enables cyanoacrylates to bond to porous surfaces Reduces frosting or fogging of the adhesive Allows cyanoacrylates to cure on strongly passivated metals, aged PVC or acidic surfaces such as on wood Typical Applications: Porous Parts Poorly Mated Parts Wire Tacking Reduction of Stress Cracking on Plastic Parts Information provided by Permabond.
Physical Properties Metric English Comments
Storage Temperature <= 27.0 °C
<= 80.6 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 9.646 - 11.024 MPa
1399 - 1598.9 psi
Steel, Shear
Thermal Properties Metric English Comments
Flash Point -4.40 °C
24.1 °F
Processing Properties Metric English Comments
Cure Time >= 0.0833 min
>= 0.00139 hour
Steel, set time
>= 0.0833 min
>= 0.00139 hour
Phenolic, set time
>= 0.167 min
>= 0.00278 hour
Buna N Rubber, set time
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Water-White
Users viewing this material also viewed the following: