ATI Allegheny Ludlum AL 22-3 Controlled Expansion Alloy

Category Metal , Superalloy , Iron Base
Manufacturer ATI Allegheny Ludlum
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allegheny Ludlum AL 22-3 Controlled Expansion Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Available in sheet and strip for use in bimetallic thermostats. ASTM B753 Type T-22Information provided by Allegheny Ludlum
Component Elements Properties Metric English Comments
Chromium, Cr 22 %
22 %
Iron, Fe 75 %
75 %
as balance
Nickel, Ni 3.0 %
3.0 %