Johnson Matthey Matti-phos 15 Alloy for Fluxless Brazing of Copper

Category Metal , Nonferrous Metal , Copper Alloy , Solder/Braze Alloy
Manufacturer Johnson Matthey
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Johnson Matthey Matti-phos 15 Alloy for Fluxless Brazing of Copper.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This alloy gives ductile joints on copper to copper and is used by electrical assemblies such as motors and contacts.Optimum Joint Gap 0.05 - 0.2 mm.AWS A5.8-92 BCuP-5BS EN 1044 1999 CP102; Does not conform exactly to the requirements of EN 1044.Federal Specification QQ-B-650 BCuP-5Equivalent to Engelhard Silvaloy 15Equivalent to Handy & Harman Sil-Fos 15Equivalent to J W Harris Stay-Silv 15Information provided by Johnson Matthey.
Thermal Properties Metric English Comments
Melting Point 645 - 800 °C
1190 - 1470 °F
Solidus 645 °C
1190 °F
Liquidus 800 °C
1470 °F
Component Elements Properties Metric English Comments
Copper, Cu 80 %
80 %
Phosphorous, P 5.0 %
5.0 %
Silver, Ag 15 %
15 %