Styron DL 447 SB Latex

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron DL 447 SB Latex.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Performance Features: Integrated antifoam, low e-modulus mortars, freeze/thaw stabilityApplications: 2K Cementious and Modified ConcreteAsia PacificInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 48.5 %
48.5 %
pH 11
11
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -17.0 °C
1.40 °F