Johnson Matthey HC Platinum w/ 5% Cobalt Jewelry Alloy

Category Metal , Nonferrous Metal , Precious Metal , Platinum Alloy
Manufacturer Johnson Matthey
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Johnson Matthey HC Platinum w/ 5% Cobalt Jewelry Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fluid for hard castings. Cobalt has been used to create casting alloys at various levels of fineness. Cobalt suppresses oxygen level in the melt, improves fluidity and castability and gives a good final hardness without reducing the melting range significantly.
Physical Properties Metric English Comments
Density 20.8 g/cc
0.751 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 135
135
Annealed
Elongation at Break 20 %
20 %
Annealed
Thermal Properties Metric English Comments
Melting Point 1750 - 1765 °C
3180 - 3209 °F
Solidus 1750 °C
3180 °F
Liquidus 1765 °C
3209 °F
Component Elements Properties Metric English Comments
Cobalt, Co 5.0 %
5.0 %
Platinum, Pt 95 %
95 %