Gwent Electronic Materials D2060131D1 Dielectric Paste

Category Fluid , Metal , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Gwent Electronic Materials D2060131D1 Dielectric Paste.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This Material is a white colored screen printable polymer dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode. It contains a crosslinking resin system for printing on substrates with low adhesion surfaces, e.g.: Polyimide. The formulation is designed for maximum flexibility. Screen Printing Equipment: semi-automatic, manualScreen Types: stainless steel, polyester, mesh 156 to 325tpiSubstrate: Polyester, PVC, Polycarbonate, or Ceramic.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 68.5 - 71.3 %

@Temperature 150 °C
68.5 - 71.3 %

@Temperature 302 °F
Viscosity 5500 - 8500 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
5500 - 8500 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Thickness 16.0 microns
0.630 mil
Using a 230 mesh stainless steel screen with 13 micron emulsion
Storage Temperature 20.0 °C
68.0 °F
sealed container
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 150 °C
0.500 hour

@Temperature 302 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 190
Using a 230 mesh stainless steel screen with 13 micron emulsion