Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) X 30 G Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) X 30 G Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
X30G is for injection molding because of its good flow properties this grade offers easy processing and extruded items exhibit high stiffness.Applications: The grade is widely used for injection molding consumer goods such as feed containers, house wares, toys, garden furniture and parts for the automotive industry.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 9.0 g/10 min
9.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 71
71
ISO 868
Tensile Stress 34.0 MPa
4930 psi
ISO R527
Elongation at Yield 13 %
13 %
ISO R527
Flexural Modulus 1.50 GPa
218 ksi
ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 155 °C
311 °F
ISO 306/A
Heat Distortion Temperature 115 °C
239 °F
ISO 75/B
Users viewing this material also viewed the following: