Moplen Z 30 G is a high flow homopolymer for injection molding and compounding applications. Moplen Z 30 G exhibits a high stiffness and an outstanding processability for shorter cycle times and easy mold filling. The product is suitable for injection moulding applications such as thin-walled containers and other general purpose packaging items, toys, vacuum flasks, household and kitchen articles . Moplen Z 30 G also is an excellent polymer base for compounding and master batches.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Stress 32.0 MPa
4640 psi
ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus 1.50 GPa
218 ksi
ASTM D790
Izod Impact, Notched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 152 °C
306 °F
ASTM D1525
Heat Distortion Temperature 94.0 °C
201 °F
ASTM D3012