Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos T50-200 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos T50-200 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ineos T50-200 is a high density polyethylene copolymer of narrow molecular weight distribution. It is intended for injection molding applications which require high impact resistance and good environmental stress crack resistance. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D4883
Environmental Stress Crack Resistance 12 hour
12 hour
Condition B, 10%; ASTM D1693
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 26.9 MPa
3900 psi
2 in/min (50 mm/min); ASTM D-638
27.6 MPa
4000 psi
ASTM D638
Elongation at Break 800.0 %
800.0 %
2 in/min (50 mm/min); ASTM D-638
Flexural Modulus 1.276 GPa
185.1 ksi
Tangent-Method 1; ASTM D790
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C
171 °F
ASTM D648
Vicat Softening Point 131 °C
268 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Descriptive Properties Value Comments