Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 3900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Multibase Multi-Pro® 3019 CXUW Polypropylene
Calcium Carbonate Filler, 30% by weight.Features:Gloss, High Impact Resistance, GoodUV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn EquipmentInformation prov..
Tensile Strength, Yield 26.9 MPa
3900 psi
2 in per min; ASTM D638
Network Polymers NPP 20-0202
Description: Random Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Petromont 1002 High Density Polyethylene Resin
Petromont HDPE 1002 is a blow moulding high-density polyethylene copolymer resin produced using the UNIPOL® Process. This multi-purpose resin can be used on intermittent and continuous extrusion bl..
Tensile Strength, Yield 26.9 MPa
3900 psi
2" (50mm) per min, Type IV; ASTM D638
Formosa Plastics Formolene® HP5221 Pipe HDPE  (discontinued **)
High Density Hexene Copolymer Formolene® HP5221 is a high performance copolymer that is designed for the most demanding requirements of corrugated pipe applications. Formolene® HP5221 meets the re..
Tensile Strength, Yield 26.9 MPa
3900 psi
2 in/min (50 mm/min); ASTM D-638
Ineos T50-200 HDPE
Ineos T50-200 is a high density polyethylene copolymer of narrow molecular weight distribution. It is intended for injection molding applications which require high impact resistance and good envir..
Tensile Strength, Yield 26.9 MPa
3900 psi
2 in/min (50 mm/min); ASTM D-638
Ineos T50-3600 HDPE
Ineos T50-3600 is a high density polyethylene copolymer of narrow molecular weight distribution used primarily for high speed injection molding of thin-walled articles. It is characterized by a hig..
Tensile Strength, Yield 26.9 MPa
3900 psi
2 in/min; ASTM D638
Ineos T50-400 HDPE
T50-400 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use p..
Tensile Strength, Yield 26.9 MPa
3900 psi
2 in/min (50 mm/min); ASTM D-638
Ineos T50-500 HDPE
Ineos T50-500 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and en..
Tensile Strength, Yield 26.9 MPa
3900 psi
2 in/min; ASTM D638
Ineos T50-500-171 Polyethylene Copolymer
This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use pro..
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
LTL Color Compounds ColorRxâ„¢ PP2-1002AF Food Grade Polypropylene Random Copolymer
An approx. 10 melt Polypropylene random copolymer with FDA food contact approval and antimicrobial protection.All information provided by LTL Color Compounders, Inc.
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
LTL Color Compounds ColorRxâ„¢ PP2-1005ARX Biocompatible, Antimicrobial Polypropylene Random Copolymer
A biocompatible approx. 10 melt Polypropylene random copolymer for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information prov..
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Lucent Polymers CPP-210 Polypropylene, 10% Calcium Carbonate Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Spartech Polypro SP-1710 Co/Pol Polyolefin Sheet
Description: Polyolefin SheetInformation provided by Spartech.
Tensile Strength, Yield 26.9 MPa
3900 psi
2" (50mm) per min; ASTM D638
Formosa Plastics Formolene® 6144O Impact Copolymer Polypropylene
Impact Copolymer for Appliance Applications Formolene® 6144O is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical property balance and excellent dimensional s..
Tensile Strength, Yield 26.9 MPa
3900 psi
2" (50mm) per min, Type IV; ASTM D638
Formosa Plastics Formolene® E602 Pipe HDPE
High Density Polyethylene High Molecular Weight Bi-Modal Resin for Non-Pressure Pipe Extrusion Applications Formolene® E602 is a high performance copolymer that is designed for the most demanding r..
Tensile Strength, Yield 26.9 MPa
3900 psi
2" (50mm) per min, Type IV; ASTM D638
Formosa Plastics Formolene® HB5202A Blow Molding HDPE
High Density Polyethylene Hexene Copolymer for Blow Molding – With Antistat Formolene® HB5202A is designed for applications requiring excellent stiffness and stress crack resistance propertiesAppl..
Tensile Strength, Yield 26.9 MPa
3900 psi
2" (50mm) per min.; ASTM D638 Type IV
Formosa Plastics Formolene® HB5202B2 Sheet and Thermoforming HDPE
High Density Polyethylene Hexene CopolymerApplications: Containers for bleach, detergents, chemicals; Molded or formed industrial housings, shrouds and tanks.Formolene HB5202B2 is designed for appli..
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Eastman Tenite 307A4000015 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Eastman Tenite 360A4861316 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Eastman Tenite 360E3V45516 Propionate Water Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Eastman Tenite 380A4000015 Cellulose Acetate Propionate, Clear, Trsp
Applications:OphthalmicsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel..
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Eastman Tenite Propionate 360E0096916 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 16%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Eastman Tenite Propionate 381E4000015 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Eastman Tenite Propionate 384A4000016 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 16%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Yield 26.9 MPa
3900 psi
molded and tested in accordance with ASTM D 4101; ASTM D638
Dow 6D20 Polypropylene Resin
DOW 6D20 is intended for use in film and extrusion blow molding processes. It is especially suited for multilayered, barrier bottles.Information provided by DowDow Announced Sale of Global Polyprop..
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Dow R131-02A Polypropylene Random Copolymer Resin
DOW R131-02A Polypropylene Resin is a random copolymer intended for use in extrusion blow molding applications. The product can be used in both single layer and multilayer designs including barrier..
Tensile Strength, Yield 26.9 MPa
3900 psi
2 in/min (50 mm/min); ASTM D-638
Bapolene® PP5026 Polypropylene, Extrusion/Injection Grade
Polypropylene extrusion impact copolymer with excellent color and processability. This resin also has a superior balance of stiffness and impact strength. This product meets FDA regulation 21 CFR ..
Tensile Strength, Yield 26.9 MPa
3900 psi
2 in/min (50 mm/min); ASTM D638
Bapolene® PP5052 Polypropylene, Injection Grade
Polypropylene injection impact copolymer with excellent color and processability. This resin also has a superior balance of stiffness and impact strength. This product meets FDA standards for food..
Tensile Strength, Yield 26.9 MPa
3900 psi
2 in/min.; ASTM D638
Ineos J50-2000-119 HDPE
HDPE J50-2000-119 is a high density, narrow molecular weight polyethylene copolymer intended for applications requiring a glossy surface finish and reasonably good impact strength and rigidity. It i..
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Techmer ES HiFill FR® HDPE FR-HB
Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc.
Copyright © lookpolymers.com All Rights Reserved