| Category | Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Transparent |
| Manufacturer | Ineos ABS |
| Trade Name | Lustran® SAN |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Ineos ABS Lustran® SAN 31 51.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.07 g/cc | 0.0387 lb/in³ | |
| Melt Flow | 21 g/10 min @Load 10.0 kg, Temperature 220 °C |
21 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min. |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 59.0 MPa | 8560 psi | |
| Elongation at Break | 3.0 % | 3.0 % | Nominal |
| Elongation at Yield | 3.0 % | 3.0 % | |
| Tensile Modulus | 3.45 GPa | 500 ksi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature 20.0 °C |
37.8 µin/in-°F @Temperature 68.0 °F |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 96.0 °C | 205 °F | |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
UL Recognized |
| HB @Thickness 3.00 mm |
HB @Thickness 0.118 in |
UL Recognized |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 80 % | 80 % | Manufacturer states transparent but does not quantify |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 240 °C | 464 °F | Injection Molding |
| Mold Temperature | 60.0 °C | 140 °F | Injection Molding |
| Injection Velocity | 200 mm/sec | 7.87 in/sec | |
| Injection Pressure | 55.0 MPa | 7980 psi |