Stir SpA SA 81 N (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Stir SpA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stir SpA SA 81 N (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Application: Extrusion coaxialInformation provided by STIR SpA
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ISO 868
Tensile Strength at Break 20.63 MPa
2992 psi
ISO R 527
Elongation at Break 369 %
369 %
ISO R 527