Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 10.75 g/cc | 0.3884 lb/in³ |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Brinell | 10 | 10 | |
Tensile Strength at Break | 30.3 MPa | 4400 psi | |
Elongation at Break | 30 % | 30 % | |
Modulus of Elasticity | 19.0 GPa | 2760 ksi | |
Shear Strength | 16.5 MPa | 2400 psi |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 29.0 µm/m-°C @Temperature 20.0 °C |
16.1 µin/in-°F @Temperature 68.0 °F |
|
Thermal Conductivity | 25.0 W/m-K @Temperature 85.0 °C |
174 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Melting Point | 275 - 302 °C | 527 - 576 °F | |
Solidus | 275 °C | 527 °F | |
Liquidus | 302 °C | 576 °F |
Component Elements Properties | Metric | English | Comments |
---|---|---|---|
Lead, Pb | 89.5 % | 89.5 % | |
Tin, Sn | 10.5 % | 10.5 % |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000193 ohm-cm | 0.0000193 ohm-cm |