| Category | Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy , Tin Alloy |
| Manufacturer | Indium Corporation of America |
| Trade Name | Indalloy |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Indium Corp. Indalloy 240 Bismuth-Lead-Tin Solder Alloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 8.97 g/cc | 0.324 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 41.4 MPa | 6000 psi | |
| Elongation at Break | 48 % | 48 % | |
| Modulus of Elasticity | 36.4 GPa | 5280 ksi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 22.0 µm/m-°C <br>@Temperature 20.0 °C |
12.2 µin/in-°F <br>@Temperature 68.0 °F |
|
| Melting Point | 160 - 173 °C | 320 - 343 °F | |
| Solidus | 160 °C | 320 °F | |
| Liquidus | 173 °C | 343 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Bismuth, Bi | 8.0 % | 8.0 % | |
| Lead, Pb | 46 % | 46 % | |
| Tin, Sn | 46 % | 46 % |