Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M Chemical GUARD DOGâ„¢ UV5411 Benzotriazole UV Absorber, Powder and LD Pellet

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer M Chemical Company, Inc.
Trade Name GUARD DOG™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF M Chemical GUARD DOGâ„¢ UV5411 Benzotriazole UV Absorber, Powder and LD Pellet.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
GUARD DOG™ UV5411 light stabilizer is a derivative of Benzotriazole that has exceptionally strong and broad-range UV absorption properties throughout the UV spectrum. It is highly recommended for thermoset plastics, organic substrates and coatings that function as ultraviolet screens for photosensitive substrates. It helps to preserve the original appearance and physical integrity of polymeric systems during outdoor weathering.Applications: Extremely effective in unsaturated polyesters (0.2 - 0.5 wt%), PVC, styrenics, acrylics, polycarbonates, PU (0.2 - 1 wt%), polyamide (0.2 - 0.5 wt%), PVB, PMMA, PE and elastomers.Performance Benefits:Strong and broad absorption of UV light in 300 - 400 nm range with low color contributionHigh degree of inherent light stability and has low volatilityExcellent compatibility with polymers and exceptional UV protection for PC and engineering polymers.Typical Properties:White crystalline free flowing powderlambda MAX, nm: 346Solubility (g/100g @ 25°C): Benzene 65, n-Butyl Acetate 245, Methylene Chloride 70.9, Styrenics 49.7, Xylene 50
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc

@Temperature 25.0 °C
1.18 g/cc

@Temperature 77.0 °F
Molecular Weight 323 g/mol
323 g/mol
Absorption Coefficient <= 49.3
<= 49.3
10 mg UV/l of Toluene
Thermal Properties Metric English Comments
Melting Point 103 - 105 °C
217 - 221 °F
Descriptive Properties Value Comments
CAS Number 3147-75-9
Molecular Formula C<sub>20</sub>H<sub>26</sub>N<sub>3</sub>O
Name 2-(2'-Hydroxy-5'-octylphenyl) benzotriazole
Recommended Dosage 0.1 - 1.0%
depending upon the substrate and performance requirements