Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Water Absorption 2.3 %

@Time 86400 sec
2.3 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0019 cm/cm

@Thickness 3.17 mm
0.0019 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 77.9 MPa
11300 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Strength 150 MPa
21700 psi
ASTM D790
Flexural Modulus 3.17 GPa
460 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm

@Thickness 3.17 mm
1.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 73.8 µm/m-°C
41.0 µin/in-°F
ASTM D696
Melting Point 146 °C
295 °F
Maximum Service Temperature, Inert 130 °C
266 °F
ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Unannealed; ASTM D648