Huntsman Araldite 94-105 Water-Based Hardener

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite 94-105 Water-Based Hardener.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Base Resin is ECN 1280. Typical Solids Content 55%. Mean Particle Size 2µm. Weight per Epoxide (EEW, g/eq), solids basis, 230 to 251.Comments/Applications: Adhesives; Fiber-Sizing; Textiles; Abrasives; Paper treatment Non-ionic character. Very high functionality. Excellent stability. Excellent temperature and chemical resistance.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 10000 - 30000 cP
10000 - 30000 cP