Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.0025 Phosphoric Acid Anodized Aluminum Honeycomb

Category Metal , Metal Foam, Mesh, or Honeycomb , Nonferrous Metal , Aluminum Alloy , 5000 Series Aluminum Alloy
Manufacturer Hexcel
Trade Name HexWeb®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.0025 Phosphoric Acid Anodized Aluminum Honeycomb.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the face sheets that carry bending loads and the honeycomb that carries the shear loads. The adhesive is the interface between the facing and the core in the same way that the oxide on the aluminum and the primer that has been applied to it is the interface between the honeycomb substrate material and the bonding adhesive. This interface is critical to the performance of honeycomb bonded assemblies.HexWeb® CR-PAA™ is designed for aircraft structures that are exposed to demanding environmental conditions. HexWeb® CR-PAA™ outperforms standard MIL-C-7438 core in salt spray and HexWeb® crack propagation tests.
Physical Properties Metric English Comments
Density 0.0833 g/cc
0.00301 lb/in³
Nominal
Mechanical Properties Metric English Comments
Compressive Yield Strength >= 3.45 MPa
>= 500 psi
Bare, min
>= 3.52 MPa
>= 510 psi
Stabilized, min
4.76 MPa
690 psi
Bare, typ
5.24 MPa
760 psi
Stabilized, typ
Compressive Modulus 1.31 GPa
190 ksi
Stabilized, typ
Shear Modulus 0.244 GPa
35.4 ksi
Plate Shear, W Direction, typ
0.565 GPa
82.0 ksi
Plate Shear, L Direction, typ
Shear Strength >= 1.38 MPa
>= 200 psi
Plate Shear, W Direction, min
1.83 MPa
265 psi
Plate Shear, W Direction, typ
>= 2.48 MPa
>= 360 psi
Plate Shear, L Direction, min
2.83 MPa
410 psi
Plate Shear, L Direction, typ