Physical Properties Metric English Comments
Melt Flow 1.7 g/10 min
1.7 g/10 min
ASTM D1238G
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Ultimate 50.0 MPa
7250 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Yield Strength 68.6 MPa
9950 psi
ASTM D790
Flexural Modulus 2.16 GPa
313 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 102 °C
216 °F
Heat Distortion Temp
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
ASTM D648
Vicat Softening Point 123 °C
253 °F
ASTM D1525