H.C. Starck Amperit® 175.1 Nickel (Ni)

Category Metal , Nonferrous Metal , Nickel Alloy , Pure Element
Manufacturer H.C. Starck
Trade Name Amperit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 175.1 Nickel (Ni).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Particle Size 22 µm
22 µm
Maximum of 15% less than
45 µm
45 µm
Maximum of 7% less than
Component Elements Properties Metric English Comments
Carbon, C <= 0.050 %
<= 0.050 %
Cobalt, Co <= 0.050 %
<= 0.050 %
Iron, Fe <= 0.10 %
<= 0.10 %
Nickel, Ni 99.74 - 100 %
99.74 - 100 %
Silicon, Si <= 0.0010 %
<= 0.0010 %
Sulfur, S <= 0.050 %
<= 0.050 %