Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast FI 55-11 Insulating Refractory Brick

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast FI 55-11 Insulating Refractory Brick.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 1.04 - 1.16 g/cc
0.0376 - 0.0419 lb/in³
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 8.00 - 12.0 MPa
1160 - 1740 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.380 - 0.580 W/m-K

@Temperature 200 °C
2.64 - 4.03 BTU-in/hr-ft²-°F

@Temperature 392 °F
0.410 - 0.610 W/m-K

@Temperature 600 °C
2.85 - 4.23 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.440 - 0.640 W/m-K

@Temperature 1000 °C
3.05 - 4.44 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1550 °C
2820 °F
Shrinkage 0.200 - 0.600 %

@Temperature 1520 °C,
Time 86400 sec
0.200 - 0.600 %

@Temperature 2770 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 57 %
57 %
Fe2O3 <= 1.5 %
<= 1.5 %
SiO2 39 %
39 %
Descriptive Properties Value Comments
Segercone 36