Ni50Mn28.5Ga21.5 single crystal. The magnetic shape memory phenomenon is produced by magnetic-field-induced rearrangement of (ferromagnetic) twinned martensite microstructure accompanied by a large macroscopic deformation. The magnetic field/strain curve can be altered by surface treatment.Applications:ActuatorsBreaker switches/fusesEnergy harvestersVibration dampersSensors
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 °C
158 °F
martensite to austenite transformation
Component Elements Properties Metric English Comments
Gallium, Ga 21.5 %
21.5 %
molar basis
Manganese, Mn 28.5 %
28.5 %
molar basis
Nickel, Ni 50 %
50 %
molar basis
Electrical Properties Metric English Comments
Curie Temperature 95.0 - 105 °C
203 - 221 °F
Descriptive Properties Value Comments
Elongation in Magnetic Field < 6%
maximum
3 to 5%
typical
Fatigue Life several hundred million cycles
Force Density 2 MPa
Magnetic Field 0.8 T
Response < 1 to 2 kHz
Work Output < 100 kJ/m<sup>3</sup>
force times stroke