| Category | Polymer , Thermoplastic , Nylon |
| Manufacturer | Arkema |
| Trade Name | PLATAMID® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Arkema Group PLATAMID® 8020 Copolyamide.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
| Moisture Absorption at Equilibrium | 0.80 % | 0.80 % | 20°C, 65% RH; ASTM D570 |
| 1.5 % | 1.5 % | 20°C, 100% RH; ASTM D570 | |
| 2.3 % | 2.3 % | 100°C, 100% RH; ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 62 | 62 | ASTM D785 |
| Tensile Strength, Ultimate | 39.0 MPa | 5660 psi | ASTM D638 |
| Elongation at Break | 200 % | 200 % | ASTM D638 |
| Flexural Modulus | 0.276 GPa | 40.0 ksi | ASTM D790 |
| 0.161 GPa @Temperature 49.0 °C |
23.3 ksi @Temperature 120 °F |
ASTM D790 | |
| 0.94975 GPa @Temperature 0.000 °C |
137.75 ksi @Temperature 32.0 °F |
ASTM D790 | |
| 1.60 GPa @Temperature -40.0 °C |
232 ksi @Temperature -40.0 °F |
ASTM D790 | |
| Izod Impact, Notched | NB | NB | ASTM D256 |
| Izod Impact, Unnotched | NB | NB | ASTM D256 |
| NB @Temperature -40.0 °C |
NB @Temperature -40.0 °F |
ASTM D256 | |
| Taber Abrasion, mg/1000 Cycles | 14 | 14 | 500g; ASTM D1044 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 172 °C | 342 °F | ASTM D789 |
| Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | ASTM D648 |
| Glass Transition Temp, Tg | 34.0 °C | 93.2 °F | |
| Flammability, UL94 | V-2 | V-2 | 0.125 inch |
| Oxygen Index | 26 % | 26 % | 0.125 inch; ASTM D2563 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 90 % | 90 % | transparent; thickness not quantified |