Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay RHODAPON® OLS Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODAPON® OLS Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Rhodapon OLS is good dispersant, wetting agent and excellent low foam detergent. It helps to reduce spots and streaksChemical Name: SODIUM OCTYL SULFATECAS: 142-31-4; 111-87-5Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: RHODAPON© OLS is recommended for applications such as: fire extinguishing foam agent, mercerizing agent for textiles, surfactant in electrolyte baths for metal cleaning and wetting agent for hard surface cleaning. In the mercerizing of grey cotton goods, RHODAPON© OLS wets efficiently and remains stable in the 20-25% caustic solutions generally used for this purpose. At levels of 1% surfactant, RHODAPON© OLS demonstrates wetting times of 6.9 seconds in 20% NaOH and 8.3 seconds in 25% NaOH. These fies represent the sinking time for a standard bundle of cotton in a caustic solution of mercerizing strength. Used as a rinse aid, RHODAPON© OLS helps dishes and glassware to drain completely, reducing spots and streaks. The low foaming characteristics of RHODAPON© OLS permit its use in automatic dishwashers or other mechanical cleaning devices where rapid agitation occurs.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 34 - 37 %
34 - 37 %
RP-0540
pH 7.5 - 8.5
7.5 - 8.5
10% Solution; RP-420
Viscosity <= 100 cP
<= 100 cP
RP-0596
Optical Properties Metric English Comments
Gardner Color Number <= 3.0
<= 3.0
RP-0138
Chemical Properties Metric English Comments
Ionic Impurities - Fe (Iron) <= 3.0 ppm
<= 3.0 ppm
O-Phenanthroline; RP-0277
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
RP-0064
Composition Active
32-34%, EQ WT 232, RP-0026
Petroleum Ether Extract
<1%, RP-210
Sodium Bicarbonate
0.25-0.45%, RP-0078
Sodium Chloride
<0.5%, RP-0098
Sodium Sulphate
<1.7%, RP-0555
Critical Micelle Concentration 0.01
Foreign Matter Free of Foreign Matter
RP-0636
HLB number 42
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved