Material Notes:
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.Designed for applications requiring good elastic recoveryRecommended for applications requiring excellent flex fatigue resistanceInformation provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 65

@Thickness 2.00 mm
65

@Thickness 0.0787 in
ISO 868
Tensile Strength at Break 7.17 MPa
1040 psi
Across Flow; ASTM D412
Tensile Strength, Ultimate 1.93 MPa
280 psi
Across Flow; ASTM D412
Elongation at Break 550 %
550 %
Across Flow; ASTM D412
Compression Set 14 %
14 %
73°F, 22 hr; ASTM D395
39 %
39 %
212°F, 22 hr; ASTM D395
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Descriptive Properties Value Comments
Change in Mass in IRM 903 Oil at 257°F for 70 hr 1.02
Color Black