ExxonMobil Exxtral™ HMU 202 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ HMU 202 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin, black colored, with high stiffness and low emissions for automotive HVAC and under-the-hood applications.Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America Features: Good Dimensional StabilityLow EmissionsLow to No FoggingLow to No OdorUltra High StiffnessUses: Automotive ApplicationsAutomotive Interior PartsAutomotive Interior TrimPaintable Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 23.0 MPa
3340 psi
ISO 527-2/50
Tensile Strength, Yield 35.0 MPa
5080 psi
ISO 527-2/50
Elongation at Break 16 %
16 %
ISO 527-2/50
Elongation at Yield 4.0 %
4.0 %
ISO 527-2/50
Tensile Modulus 3.00 GPa
435 ksi
Secant; ISO 527-2
Charpy Impact, Notched 0.294 J/cm²

@Temperature 22.8 °C
1.40 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75-2/A