Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Exxtral™ CMU 201 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF ExxonMobil Exxtral™ CMU 201 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin designed for automotive interior covered applications such as retainers in which a good stiffness toughness balance is required.Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America Features: Balanced Stiffness/ToughnessGood Creep ResistanceGood Dimensional StabilityGood Mold ReleaseLow Warpage Uses: Automotive ApplicationsAutomotive Interior PartsAutomotive Interior Trim Automotive Under the Hood Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 19.0 MPa
2760 psi
ISO 527-2/50
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527-2/50
Elongation at Break 23 %
23 %
ISO 527-2/50
Elongation at Yield 3.0 %
3.0 %
ISO 527-2/50
Tensile Modulus 2.35 GPa
341 ksi
Secant; ISO 527-2/50
Charpy Impact, Notched 0.294 J/cm²

@Temperature -20.0 °C
1.40 ft-lb/in²

@Temperature -4.00 °F
Complete Break; ISO 179
0.315 J/cm²

@Temperature 0.000 °C
1.50 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
0.462 J/cm²

@Temperature 22.8 °C
2.20 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75-2/A