Material Notes:
Star C BX06008 is a 20% Carbon Fiber Reinforced ABS Injection Molding ResinInformation provided by Eurostar.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm

@Thickness 4.00 mm
0.0020 - 0.0030 in/in

@Thickness 0.157 in
E2P method
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
5 mm/min; ISO 527
Elongation at Break 1.0 %
1.0 %
5 mm/min; ISO 527
Tensile Modulus 6.60 GPa
957 ksi
1 mm/min; ISO 527
Flexural Yield Strength 105 MPa
15200 psi
2 mm/min; ISO 178
Flexural Modulus 6.50 GPa
943 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80x10x4; ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257
Processing Properties Metric English Comments
Zone 1 205 - 215 °C
401 - 419 °F
Zone 2 245 - 255 °C
473 - 491 °F
Zone 3 255 - 265 °C
491 - 509 °F
Melt Temperature 260 °C
500 °F
Mold Temperature 40.0 - 70.0 °C
104 - 158 °F
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour