Ecomass® 1080BI64 Filled Polyamide

Category Polymer , Thermoplastic , Nylon
Manufacturer Ecomass Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ecomass® 1080BI64 Filled Polyamide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Nontoxic alternative compound for weighting, balancing and radiation shielding applicationsModerate Specific GravityFilled Polyamide (PA) AlloyExcellent ToughnessInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 2.00 g/cc
2.00 g/cc
ASTM D792
Linear Mold Shrinkage 0.0070 - 0.0080 cm/cm
0.0070 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 41.4 MPa
6000 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Tensile Modulus 4.48 GPa
650 ksi
ASTM D638
Flexural Strength 62.1 MPa
9000 psi
ASTM D790
Flexural Modulus 3.79 GPa
550 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm
2.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
225 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 204 - 254 °C
400 - 490 °F
Mold Temperature 57.2 - 82.2 °C
135 - 180 °F
Drying Temperature 73.9 °C
165 °F
Dry Time 4 hour
4 hour