ChevronTexaco ISO 32 Refrigeration Oil WF

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco ISO 32 Refrigeration Oil WF.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesChevron Refrigeration Oils WF are manufactured using medium viscosity index straight mineral oils. The base stocks are carefully selected to assure the low pour points that are necessary for refrigeration compressor lubricants.Chevron Refrigeration Oils WF are highly refined and specially treated to resist the sludging action of refrigerants in the presence of high temperature and metal catalysts.These oils are water-free, which prevents carry-over oil from icing in the refrigeration expansion valves. The oils are wax-free, allowing full flow through filters, strainers, and close tolerance valves. Being wax-free (very low floc point2) assures excellent fluidity at low temperatures, meaning reduced wear and longer equipment life.Chevron Refrigeration Oils WF provide maximum wear protection to any refrigeration compressor or system in which they are used.ApplicationsChevron Refrigeration Oils WF are suitable for use in any refrigeration system, except those using HFC Freon replacement refrigerants.The viscosity grade for the application should be based on the equipment manufacturers recommendation. They are particularly suitable for Freon in the modern, compact, high pressure refrigeration systems. Since they are wax-free, they are suitable for use in very cold ambient temperatures as a bearing lubricant or for hand oiling.Chevron Refrigeration Oils WF ISO 32 and ISO 68 satisfy the requirements of hermetically sealed air conditioning compressors or the many types of smaller units.Chevron`s primary recommendation for ammonia systems is Chevron Ammonia Refrigeration Oil. Chevron Refrigeration Oils WF are registered with NSF and are acceptable as lubricants where there is no possibility of food contact (H2) in and around food processing areas. The NSF Nonfood Compounds Registration Program is a continuation of the USDA product approval and listing program, which is based on meeting regulatory requirements of appropriate use, ingredient review and labeling verification.
Physical Properties Metric English Comments
API Gravity 24 °
24 °
Saybolt Viscosity at 100°F 154 SUS
154 SUS
Saybolt Viscosity at 210°F 41 SUS
41 SUS
Kinematic Viscosity at 40°C (104°F) 29.5 cSt
29.5 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 4.3 cSt
4.3 cSt
ASTM D445
Thermal Properties Metric English Comments
Pour Point -40.0 °C
-40.0 °F
ASTM D97
Flash Point 168 °C
334 °F
ASTM D92
Electrical Properties Metric English Comments
Dielectric Strength 1.18 kV/mm
30.0 kV/in
Descriptive Properties Value Comments
Color 1
Floc Point, °C -54