Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.00 J/g-°C | 0.478 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Cycoloy® EHA PC+ABS PC+ABS. Electroplateable. |
|||
Specific Heat Capacity | 2.00 J/g-°C @Temperature 280 °C |
0.478 BTU/lb-°F @Temperature 536 °F |
DSC |
Eastman Heatwave CF746 Polymer
(discontinued **) Heatwave is a clear, reheat enhanced, PET polyester designed for heatset containers containing a UV light protection package chemically bound to the backbone of the polymer. Pellets are 2.5 mm (0.1 .. |
|||
Specific Heat Capacity | 2.00 J/g-°C @Temperature 280 °C |
0.478 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman Aqua 18696 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Containers made from 186.. |
|||
Specific Heat Capacity | 2.00 J/g-°C @Temperature 200 °C |
0.478 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman 9921P PET Film
(discontinued **) Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia.. |
|||
Specific Heat Capacity | 2.00 J/g-°C @Temperature 280 °C |
0.478 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman A12 PET
(discontinued **) Voridian Polymer A12 is currently produced to Eastman`s specifications and quality requirements by several resin manufacturers located in the Asis Pacific Region. Voridian Polymer A12 is available i.. |
|||
Specific Heat Capacity | 2.00 J/g-°C @Temperature 200 °C |
0.478 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman CB11E PET
(discontinued **) VORIDIAN PET CB11E is designed specifically for the carbonated soft drink (CSD) and other beverage markets in the European market area. The polymer delivers faster, more efficient processing and bet.. |
|||
Specific Heat Capacity | 2.00 J/g-°C @Temperature 280 °C |
0.478 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman CM01 PET
(discontinued **) Voridian Polymer CM01 is clear polymer that is available in North America. This product is useful for production of beverage, food, and edible oil containers.Applications/UsesCarbonated soft drink c.. |
|||
Specific Heat Capacity | 2.00 J/g-°C @Temperature 280 °C |
0.478 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman GP800 PET
(discontinued **) Voridian PET GP800 is a general purpose polymer that is available in the European, Middle East and Africa region. This product is developed for optimal production of PET bottles, containers, and fil.. |
|||
Specific Heat Capacity | 2.00 J/g-°C | 0.478 BTU/lb-°F | |
Americas Styrenics Styron® XL-8028 High Impact Polystyrene
(discontinued **) STYRON® XL-8028 high impact polystyrene is designed for VCR cassettes, toys, small appliances, telephones, housewares, tool items, computer consoles and bodies for computer cartridges. It offers hi.. |
|||
Specific Heat Capacity | 2.00 J/g-°C | 0.478 BTU/lb-°F | |
Micropol Isoplas P471 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Specific Heat Capacity | 2.00 J/g-°C | 0.478 BTU/lb-°F | |
Styron Magnum™ 342EZ ABS, Medium Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Specific Heat Capacity | 2.00 - 2.40 J/g-°C @Temperature 200 °C |
0.478 - 0.574 BTU/lb-°F @Temperature 392 °F |
DSC |
Wacker Silicones Geniomer® 140 Silicone TPE SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |
|||
Specific Heat Capacity | 2.00 - 2.40 J/g-°C @Temperature 200 °C |
0.478 - 0.574 BTU/lb-°F @Temperature 392 °F |
DSC |
Wacker Silicones Geniomer® 200 Silicone TPE Elastomer SLM TPSE 200 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |
|||
Specific Heat Capacity | 2.00 J/g-°C | 0.478 BTU/lb-°F | DSC |
Total 3802 Blue MDPE pipe, injection molding FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth.. |
|||
Specific Heat Capacity | 2.00 J/g-°C | 0.478 BTU/lb-°F | DSC |
Total 3802 YCF MDPE pipe grade FINATHENE® 3802 Y CF is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Y CF is a yellow cadmi.. |
|||
Specific Heat Capacity | 2.00 J/g-°C | 0.478 BTU/lb-°F | DSC |
Total HP 401 MDPE, pipe, cable, sheet FINATHENE® HP 401 is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® HP 401 is a black high densit.. |
|||
Specific Heat Capacity | 2.00 J/g-°C | 0.478 BTU/lb-°F | DSC |
Total Xsene® XS10 B HDPE, pipe, injection molding FINATHENE® XS10 B is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS10 B is a high performance black compound speci.. |
|||
Specific Heat Capacity | 2.00 J/g-°C | 0.478 BTU/lb-°F | DSC |
Total Xsene® XS10 H HDPE, pipe, injection molding FINATHENE® XS 10 H is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS 10 H is a high performance dark blue compound.. |
|||
Specific Heat Capacity | 2.00 J/g-°C @Temperature 200 °C |
0.478 BTU/lb-°F @Temperature 392 °F |
DSC |
Eastman Eastobond 19411 Copolyester, Film Eastobond 19411 is a terephthalate-based copolyester which is amorphous. It offers excellent organoleptic and gas-barrier properties. Eastobond 19411 has low postextrusion crystallinity and a low so.. |
|||
Specific Heat Capacity | 2.00 J/g-°C @Temperature 200 °C |
0.478 BTU/lb-°F @Temperature 392 °F |
DSC |
Eastman Eastobond 19412 Copolyester, Film Eastobond 19412 is a terephthalate-based copolyester. It is identical to our 19411 resin in every aspect, except that the 19412 has been crystallized for drying purposes and ease of handling. Eastob.. |
|||
Specific Heat Capacity | 2.00 J/g-°C @Temperature 150 °C |
0.478 BTU/lb-°F @Temperature 302 °F |
DSC |
Eastman Neostar FN005 Elastomer Neostar FN005 elastomer is a tough, clear, durable copolyester ether. It was designed for use in the profile and automotive markets, but is also used in packaging and tubing applications where tough.. |
|||
Specific Heat Capacity | 2.00 J/g-°C @Temperature 150 °C |
0.478 BTU/lb-°F @Temperature 302 °F |
DSC |
Eastman Neostar FN006 Elastomer Neostar FN006 elastomer is the second in Eastman’s series of tough, clear, durable copolyester ethers. Developed for use in the profile and automotive markets, it can also be used in packaging and .. |
|||
Specific Heat Capacity | 2.00 J/g-°C @Temperature 150 °C |
0.478 BTU/lb-°F @Temperature 302 °F |
DSC |
Eastman Neostar FN007 Elastomer Neostar FN007 elastomer is the third in Eastman’s series of tough, clear, durable copolyester ethers. Though originally designed for use in the profile and automotive markets, this innovative copol.. |
|||
Specific Heat Capacity | 2.00 J/g-°C | 0.478 BTU/lb-°F | of Liquid |
BASF Methyl Acrylate Formula: C4H6O2CAS: 96-33-3Description: Acrylic ester for manufacturing polymers and for use as a feedstock for syntheses. Applications: Methyl acrylate forms homopolymers and copolymers. Copolymer.. |
|||
Specific Heat Capacity | 2.00 J/g-°C | 0.478 BTU/lb-°F | DSC |
Total Lacqtene® 2001 TBK 46 HDPE pipe
(discontinued **) LACQTENE® 2001 TBK 46 is a high density polyethylene produced by the gas phase polymerization process. LACQTENE® 2001 TBK 46 is a black compound especially developed for pressure pipe for gas and .. |
|||
Specific Heat Capacity | 2.00 J/g-°C | 0.478 BTU/lb-°F | DSC |
Total Xsene® XS10 Orange YCF HDPE, pipe FINATHENE® XS 10 ORANGE YCF is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS 10 ORANGE YCF is a high performance .. |
|||
Specific Heat Capacity | 2.00 J/g-°C | 0.478 BTU/lb-°F | Melt value |
BASF Capron® 8260 40% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8260 is a 40% mineral reinforced polyamide 6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability includi.. |
|||
Specific Heat Capacity | 2.00 - 2.40 J/g-°C @Temperature 200 °C |
0.478 - 0.574 BTU/lb-°F @Temperature 392 °F |
DSC |
Wacker Silicones Geniomer® 80 Silicone TPE SLM TPSE 80 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |
|||
Specific Heat Capacity | 2.00 J/g-°C @Temperature 280 °C |
0.478 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman VersaTray 12822 Plastic
(discontinued **) VersaTray plastic 12822 is a polyethylene terephthalate resin designed for use as a base resin for crystallized PET (CPET) food trays and other high temperature food packaging applications. CPET foo.. |
|||
Specific Heat Capacity | 2.00 - 2.40 J/g-°C @Temperature 200 °C |
0.478 - 0.574 BTU/lb-°F @Temperature 392 °F |
DSC |
Wacker Silicones Geniomer® 60 Silicone TPE SLM TPSE 60 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |