Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eagle Brass 102 OF COPPER (Non-Certified), 1/2 Hard

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer Eagle Brass Company
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Eagle Brass 102 OF COPPER (Non-Certified), 1/2 Hard.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance and is used for high current applications.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.94 g/cc
0.323 lb/in³
Annealed
Mechanical Properties Metric English Comments
Hardness, Rockwell 30T 43 - 57
43 - 57
Thickness > 0.020 Inch
Tensile Strength, Ultimate 255 - 317 MPa
37000 - 46000 psi
Tensile Strength, Yield 207 - 303 MPa
30000 - 44000 psi
0.2% offset
Elongation at Break 8.0 - 32 %
8.0 - 32 %
in 2 in.
Tensile Modulus 117 GPa
17000 ksi
Thermal Properties Metric English Comments
CTE, linear 17.6 µm/m-°C

@Temperature 20.0 - 300 °C
9.80 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 390.8 W/m-K
2712 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu >= 99.9 %
>= 99.9 %
Oxygen, O <= 0.0010 %
<= 0.0010 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000176 ohm-cm
0.00000176 ohm-cm
Annealed