ExxonMobil Santoprene® 253-50W232 Thermoplastic Vulcanizate  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 253-50W232 Thermoplastic Vulcanizate  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A hard, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and is formulated to replace thermoset rubbers such as EPDM, polychloroprene and chlorosulphonated polyethylene. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.Key Features:Recommended for applications requiring excellent flex fatigue resistance.Recommended for applications requiring excellent ozone resistance.EU and China RoHS compliant.Uses: Automotive ApplicationsCable JacketingElectrical/Electronic ApplicationsWire & Cable Applications Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792 and ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore D 51

@Thickness 50.8 mm,
Temperature 23.0 °C
51

@Thickness 2.00 in,
Temperature 73.4 °F
ISO 868
Tensile Strength, Yield 10.9 MPa
1580 psi
Across Flow; ASTM D638
Elongation at Yield 20 %
20 %
Across Flow; ASTM D638
Thermal Properties Metric English Comments
Oxygen Index 26 %
26 %
ASTM D2863 and ISO 4589-2
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F