DuPont Fusabond® MX110D Linear Low Density Polyethylene  (discontinued **)

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Fusabond® MX110D Linear Low Density Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Typical Use: CompatibilizerCoupling agent for nonhalogen, flame retarded wire and cable compounds containing fillers such as aluminum trihydrate or magnesium hydroxideNatural fiber wood-plastic compoundsAvailability: North AmericaInformation provided by DuPont.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
Melt Flow 23 g/10 min
23 g/10 min
Thermal Properties Metric English Comments
Melting Point 122 °C
252 °F
Descriptive Properties Value Comments
MAH Graft Level, wt% High
FTIR (DuPont)