Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Mylar® 75 OL Polyester Film, 75 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Mylar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Mylar® 75 OL Polyester Film, 75 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by DuPont Packaging Polymers.An exceptionally strong polyester film designed to package foods. The film is suitable for heating food products in microwave or conventional ovens. Can be used to package, distribute, and heat foods up to 204°C (400°F).
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Average value for Mylar® films.
Moisture Vapor Transmission 0.600 cc-mm/m²-24hr-atm
1.52 cc-mil/100 in²-24hr-atm
ASTM 1249
Water Vapor Transmission 30.0 g/m²/day
1.93 g/100 in²/day
ASTM 1249
Oxygen Transmission 2.10 cc-mm/m²-24hr-atm
5.33 cc-mil/100 in²-24hr-atm
or 110 cc/m²-24hr-atm for the film. ASTM D3985
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 130 %
130 %
ASTM D882
Film Elongation at Break, TD 100 %
100 %
ASTM D882
Modulus of Elasticity 3.79 GPa
550 ksi
(stiffness), ASTM D882
Tear Strength Test 400
400
Graves, g; ASTM D1004
Seal Strength 247 g/25 mm
247 g/in
Film Tensile Strength at Break, MD 200 MPa
29000 psi
ASTM D882
Film Tensile Strength at Break, TD 242 MPa
35100 psi
ASTM D882
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Foods can be heated or cooked up to this temperature.
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved