Material Notes:
Features: This high molecular weight, hexane copolymer is tailored for light-weight blow-molded containers that require: Good stiffness and Excellent processabilityAdditives: Anti-OxidantsApplication: Bottles for detergents, Household and industrial chemical containers.CAS No. 9002-88-4Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity >= 0.961 g/cc
>= 0.961 g/cc
ASTM D1505
Environmental Stress Crack Resistance >= 20 hour
>= 20 hour
F50; ASTM D1693
Melt Flow 0.14 - 0.22 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.14 - 0.22 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.4 MPa
4410 psi
50 mm/min; ASTM D638
Elongation at Break >= 800 %

@Thickness 50.0 mm
>= 800 %

@Thickness 1.97 in
ASTM D638
Flexural Modulus 1.27 GPa
185 ksi
ASTM D790
Izod Impact, Unnotched >= 1.96 J/cm

@Temperature 23.0 °C
>= 3.67 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 133 °C
271 °F
10°C/min; ASTM D3418
Vicat Softening Point 125 °C
257 °F
ASTM D1525