Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Parker Chomerics SOFT-SHIELD® 2000 Low Closure Force, Foam Core EMI Gasket

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Parker Chomerics
Trade Name SOFT-SHIELD®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics SOFT-SHIELD® 2000 Low Closure Force, Foam Core EMI Gasket.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: SOFT-SHIELD® 2000 Series gaskets consist of silver-plated nylon yarn knitted as the outer layer over a highly compressible, thermoplastic EPDM foam core. Through a special treatment process, the yarn jacket is secured to the core. This self-terminating outer layer eliminates the need for secondary termination efforts and metal particle debris associated with the cut ends of common wire mesh gaskets. SOFT-SHIELD® 2000 Series gaskets are designed specifically for use in commercial electronic enclosures and metalized plastic housings.Information provided by Chomerics
Physical Properties Metric English Comments
Deformation 10 %
10 %
0.20 ppi
20 %
20 %
0.37 ppi
30 %
30 %
0.50 ppi
40 %
40 %
0.80 ppi
50 %
50 %
1.30 ppi
Mechanical Properties Metric English Comments
Compression Set <= 25 %

@Temperature 70.0 °C,
Time 79200 sec
<= 25 %

@Temperature 158 °F,
Time 22.0 hour
50% deflection
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Shielding Effectiveness 65 dB

@Frequency 1.00e+10 Hz
65 dB

@Frequency 1.00e+10 Hz
70 dB

@Frequency 1.00e+9 Hz
70 dB

@Frequency 1.00e+9 Hz
78 dB

@Frequency 2.00e+7 Hz
78 dB

@Frequency 2.00e+7 Hz
90 dB

@Frequency 4.00e+9 Hz
90 dB

@Frequency 4.00e+9 Hz
95 dB

@Frequency 1.00e+8 Hz
95 dB

@Frequency 1.00e+8 Hz
Users viewing this material also viewed the following: