| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | Karina Indústria e Comércio de Plásticos |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Karina 951-35/4-IS-LMP Ivory PVC Compound.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.29 - 1.35 g/cc | 1.29 - 1.35 g/cc | ASTM D 792 |
| ASTM Color | -1.73 - 1.27 | -1.73 - 1.27 | Color A, ME 12 |
| 7.91 - 10.91 | 7.91 - 10.91 | Color B, ME 12 | |
| 86.9 - 89.9 | 86.9 - 89.9 | Color L, ME 12 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 92 - 96 <br>@Time 15.0 sec |
92 - 96 <br>@Time 0.00417 hour |
ASTM D 2240 |
| Hardness, Shore D | 61 - 65 <br>@Time 15.0 sec |
61 - 65 <br>@Time 0.00417 hour |
ASTM 2240 |
| Tensile Strength | >= 12.6 MPa | >= 1820 psi | NBR NM-IEC 60811-1-1 |
| >= 12.6 MPa | >= 1820 psi | After 168 H in Air Oven at 100°C; NBR NM-IEC 60811-1-2 | |
| Elongation at Break | >= 125 % | >= 125 % | NBR NM-IEC 60811-1-1 |
| >= 125 % | >= 125 % | After 168H in Air Oven at 100°C; NBR NM-IEC 60811-1-2 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Oxygen Index | >= 23 % | >= 23 % | NBR 6245 |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Cadmium, Cd | <= 0.0050 % | <= 0.0050 % | IEC 62321 |
| Chromium, Cr | <= 0.010 % | <= 0.010 % | IEC 62321 |
| Lead, Pb | <= 0.010 % | <= 0.010 % | IEC 62321 |
| Mercury, Hg | <= 0.010 % | <= 0.010 % | IEC 62321 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 6.00e+14 ohm-cm | >= 6.00e+14 ohm-cm | ASTM D 257 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Application | CI/CCI | |
| Bromine, Br (%) | < 0.01 | IEC 62321 |
| Maximum Variation of Elongation (%) | 40 | NBR NM-IEC 60811-1-2 |
| Maximum Variation of Tensile Strength (%) | 20 | NBR NM-IEC 60811-1-2 |