Price EMAIL US    sales@lookpolymers.com
Material Notes:
40 Shore D High Performance Polyester Elastomer Developed for the Healthcare Industry Hytrel SC948 NC010 is a low modulus grade with nom. durometer hardness of 40D contains non-discoloring stabilizer and can be processed by various thermoplastic procesInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore D <= 40
<= 40
ISO 868
Tensile Strength at Break 22.0 MPa
3190 psi
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Tensile Modulus 0.0300 GPa
4.35 ksi
ISO 527-1/-2
Charpy Impact, Notched NB
NB
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 193 °C
379 °F
10°C/min; ISO 11357-1/-3
Descriptive Properties Value Comments
Delivery Form Pellets
Part Marking Code >TPC-ET<
ISO 11469
Processing Casting
Film Extrusion
Injection Moulding
Other Extrusion
Profile Extrusion
Sheet Extrusion
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification TPC-ET
ISO 1043
Special Characteristics Light stabilised or stable to light