| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 40.0 - 80.0 °C | 104 - 176 °F | Average value: 56.9 °C Grade Count:22 |
|
Overview of materials for EMAAA Terpolymer
This property data is a summary of similar materials in the MatWeb database for the category "EMAAA Terpolymer". Each property range of values reported is minimum and maximum values of appropriate M..
|
|||
| Vicat Softening Point | 40.0 - 81.0 °C | 104 - 178 °F | Average value: 58.9 °C Grade Count:45 |
|
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported..
|
|||
| Vicat Softening Point | 40.0 - 181 °C | 104 - 358 °F | Average value: 63.9 °C Grade Count:62 |
|
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported ..
|
|||
| Vicat Softening Point | 40.0 °C | 104 °F | Rate B; ASTM D-1525 |
|
ExxonMobil Iotek® 7510 Zinc Ionomer Molding/Extrusion Resin
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A "soft" zinc ionomer with excellent flexibility and impact strength. This ionomer has outstanding adhesion to glass, metals and paper. IOTEK iono..
|
|||
| Vicat Softening Point | 40.0 °C | 104 °F | Rate B; ASTM D-1525 |
|
ExxonMobil Iotek® 7520 Zinc Ionomer Molding/Extrusion Resin
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A "soft" zinc ionomer with excellent flexibility and impact strength. This ionomer has outstanding adhesion to glass, metals and paper. IOTEK iono..
|
|||
| Vicat Softening Point | 40.0 °C | 104 °F | ASTM D1525 |
|
DuPont Elvax® 3185 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
33 wt% Vinyl Acetate.Elvax® 3185 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins..
|
|||
| Vicat Softening Point | 40.0 °C | 104 °F | ASTM D1525 |
|
ExxonMobil Escorene™ UL 7741 Ethylene Vinyl Acetate Copolymer
Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsIndustrial SealantsHot Melt AdhesivesWax Blends..
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 1.02 kg |
<=
104
°F @Load 2.25 lb |
ASTM D1525 |
|
Arkema Group LOTRYL® 28 MA 07 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 28 MA 07 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 28 MA 07 is a polyme..
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 1.02 kg |
<=
104
°F @Load 2.25 lb |
ASTM D1525 |
|
Arkema Group LOTRYL® 37 EH 175 Copolymer Ethylene - 2-Ethylhexyl Acrylate
LOTRYL® 37EH175 is a random copolymer of Ethylene and 2-Ethylhexyl Acrylate, prepared by the high pressure polymerization process. LOTRYL® 37EH175 is particularly recommended for the formulation o..
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 0.999 kg |
<=
104
°F @Load 2.20 lb |
ASTM D1525 |
|
Arkema Group LOTRYL® 37 EH 550 Copolymer Ethylene - Acrylic Ester
LOTRYL 37 EH 550 is a random copolymer of Ethylene and 2-Ethylhexyl Acrylate, prepared by the high pressure polymerization process. Co-monomer content is 37% in weight. LOTRYL 37 EH 550 is particula..
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 1.02 kg |
<=
104
°F @Load 2.25 lb |
ASTM D1525 |
|
Arkema Group LOTRYL® Bestpeel 2407 Copolymer Ethylene - Methyl Acrylate
LOTRYL® Bestpeel 2407 is a ready-to-use thermoplastic composition designed to make peelable heat seal layers onto various substrates. The base resin is a random copolymer of ethylene and methyl acr..
|
|||
| Vicat Softening Point | <= 40.0 °C | <= 104 °F | ASTM D1525 |
|
Arkema Group Orevac® 9305 Film EVA-MAH Terpolymer
EVA Terpolymers based Main Application: Hot melt adhesivesInformation provided by Arkema Group
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 0.999 kg |
<=
104
°F @Load 2.20 lb |
ASTM D1525 |
|
Arkema Group BONDINE® HX 8290 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
BONDINE® HX 8290 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. This grade is characterised by a high fluidity. Due..
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 0.999 kg |
<=
104
°F @Load 2.20 lb |
ISO 306 |
|
Arkema Group EVATANE® 28-150 Copolymer Ethylene - Vinyl Acetate
EVATANE® 28-150 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-150 is stabilized with antioxidants. The High Vinyl Acetate ..
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 0.999 kg |
<=
104
°F @Load 2.20 lb |
ISO 306 |
|
Arkema Group EVATANE® 28-40 Copolymer Ethylene - Vinyl Acetate
EVATANE® 28-40 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-40 is stabilized with antioxidants. The High Vinyl Acetate co..
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 0.999 kg |
<=
104
°F @Load 2.20 lb |
ISO 306 |
|
Arkema Group EVATANE® 33-15 Copolymer Ethylene - Vinyl Acetate
EVATANE® 33-15 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-15 is stabilized with antioxidants. The High Vinyl Acetate co..
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 0.999 kg |
<=
104
°F @Load 2.20 lb |
ISO 306 |
|
Arkema Group EVATANE® 33-25 Copolymer Ethylene - Vinyl Acetate
EVATANE® 33-25 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-25 is stabilized with antioxidants. The High Vinyl Acetate co..
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 0.999 kg |
<=
104
°F @Load 2.20 lb |
ISO 306 |
|
Arkema Group EVATANE® 33-400 Copolymer Ethylene - Vinyl Acetate
EVATANE® 33-400 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-400 is stabilized with antioxidants. The High Vinyl Acetate ..
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 0.999 kg |
<=
104
°F @Load 2.20 lb |
ISO 306 |
|
Arkema Group EVATANE® 33-45 Copolymer Ethylene - Vinyl Acetate
EVATANE® 33-45 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-45 is stabilized with antioxidants. The High Vinyl Acetate co..
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 1.02 kg |
<=
104
°F @Load 2.25 lb |
ISO 306 |
|
Arkema Group EVATANE® 40-55 Copolymer Ethylene - Vinyl Acetate
EVATANE® 40-55 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. It’s stabilized with antioxidants and contains slip and antiblock additiv..
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 1.02 kg |
<=
104
°F @Load 2.25 lb |
ISO 306 |
|
Arkema Group EVATANE® 42-60 Copolymer Ethylene - Vinyl Acetate
EVATANE 42-60 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE 42-60 is stabilized with antioxidants and contains slip and antibloc..
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 0.999 kg |
<=
104
°F @Load 2.20 lb |
ASTM D1525 |
|
Arkema Group LOTADER® 4700 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 4700 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Comonomer content is high. Due to its properties (reacti..
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 0.999 kg |
<=
104
°F @Load 2.20 lb |
ASTM D1525 |
|
Arkema Group LOTADER® 4720 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 4720 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Comonomer content is high. Due to its properties (reacti..
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 0.999 kg |
<=
104
°F @Load 2.20 lb |
ASTM D1525 |
|
Arkema Group LOTADER® AX 8900 Terpolymer Ethylene - Acrylic Ester - Glycidyl Methacrylate
LOTADER® AX 8900 is a random terpolymer of ethylene, acrylic ester and glycidyl methacrylate, polymerized under high pressure in an autoclave process. Comonomer content is high. Due to its properti..
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 0.999 kg |
<=
104
°F @Load 2.20 lb |
ISO 306 |
|
Arkema Group EVATANE® 18-500 Copolymer Ethylene - Vinyl Acetate
EVATANE® 18-500 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 18-500 is stabilized with antioxidants. The High Vinyl Acetate ..
|
|||
| Vicat Softening Point |
40.0
°C @Load 0.999 kg |
104
°F @Load 2.20 lb |
ISO 306 |
|
Arkema Group EVATANE® 28-05 Copolymer Ethylene - Vinyl Acetate
EVATANE® 28-05 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-05 is stabilized with antioxidants. The High Vinyl Acetate co..
|
|||
| Vicat Softening Point |
<=
40.0
°C @Load 1.02 kg |
<=
104
°F @Load 2.25 lb |
ISO 306 |
|
Arkema Group EVATANE® 28-420 Copolymer Ethylene - Vinyl Acetate
EVATANE® 28-420 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-420 is stabilized with antioxidants. The High Vinyl Acetate ..
|
|||
| Vicat Softening Point |
40.0
°C @Load 5.10 kg |
104
°F @Load 11.2 lb |
ISO 306 |
|
Borealis Daplen™ EF103AE Polypropylene TPO Compound
Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an..
|
|||
| Vicat Softening Point | 40.0 - 74.0 °C | 104 - 165 °F | Average value: 60.4 °C Grade Count:39 |
|
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..
|
|||
| Vicat Softening Point | 40.0 °C | 104 °F | ASTM D1525, ISO 306 |
|
DuPont Elvax® 240 Ethylene Vinyl Acetate
(discontinued **)
DuPont™ Elvax® 240 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 240 resins can be used for the following applications: adhesives, sealants,..
|
|||