Dow Tyrin® CM0136 Formulation

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Dow Chemical
Trade Name Tyrin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Tyrin® CM0136 Formulation.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FormulationTyrin® CPE Elastomer
Physical Properties Metric English Comments
Mooney Viscosity >= 38

@Temperature 121 °C
>= 38

@Temperature 250 °F
ML 1 + 4; ASTM D1646
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
ASTM D2240
Tensile Strength, Ultimate 20.7 MPa
3000 psi
ASTM D412
Elongation at Break 310 %
310 %
ASTM D412
200% Modulus 0.0117 GPa
1.70 ksi
ASTM D412