Lucite International Elvacite ® 2552 Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Elvacite ®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Elvacite ® 2552 Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Elvacite® 2552 is a solid bead thermoplastic methacrylate copolymer intended for use in solvent based coating systems where high gloss and apparent depth of finish are important. This specially designed polymer is internally plasticized to resist cold cracking and crazing and to provide flexibility over a broad range of temperatures. Elvacite® 2552 exhibits excellent outdoor durability and resistance to ultraviolet degradation and chemical attack from solvents such as alcohol or gasoline.The resin may be used in refinish applications and transportation finishes such as automotive, motorcycle, and bicycle in multiple coats as a high gloss clear top coat, or as the main binder in high gloss glamour type pigmented base coats. Elvacite® 2552 demonstrates excellent adhesion to plastic substrates such as PS, ABS, and PVC as well as interlayer integrity and adhesion in multiple coat applications used to achieve depth. Solvent systems containing alcohol, methyl ethyl ketone, and toluene work well with Elvacite® 2552 whether the coating is applied mechanically or as an aerosol.Information provided by Lucite International
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
Density 1.079 g/cc
0.03898 lb/in³
Brookfield Viscosity 1100 cP

@Temperature 25.0 °C
1100 cP

@Temperature 77.0 °F
in Toluene, 37.5% solids
2250 cP

@Temperature 25.0 °C
2250 cP

@Temperature 77.0 °F
in Toluene, 40.0% solids
Viscosity Measurement 0.33
0.33
Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 75000 g/mol
75000 g/mol
Mechanical Properties Metric English Comments
Hardness, Knoop 15.5
15.5
Tukon Hardness
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 90.0 °C
194 °F
Chemical Properties Metric English Comments
Total Acid Number 0.00
0.00