Trelleborg AEM Eccofloat® EL-34/6000 Syntactic Foam

Category Polymer
Manufacturer Trelleborg AEM
Trade Name Eccofloat®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg AEM Eccofloat® EL-34/6000 Syntactic Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EL Grade epoxy syntactic foams are the material of choice for manufacturing manned and unmanned submersibles because of their density range and ability to withstand exposure to diesel fuels and hydraulic fluids.These composite foams provide ultra low densities by selecting only the highest specification hollow glass microspheres, called Eccospheres®, and combining them within a rigid, high strength resin system. The syntactic foam is typically cast into blocks and then is used to prepare large buoyancy modules that can be readily shaped to conform to hull contours and outfitted for installation in the forward and aft free-flood areas of submarines.Information provided by Trelleborg AEM.
Physical Properties Metric English Comments
Density 0.545 g/cc
0.0197 lb/in³
Mechanical Properties Metric English Comments
Compressive Strength 62.1 MPa
9000 psi
Service Pressure
Descriptive Properties Value Comments
Service Depth 20,000 FSW
Depth Below Sea Level - Feet
6000 MSW