Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

American Polymers API 545 Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer American Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Polymers API 545 Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
API 545 is a high impact, high heat resistant grade of impact modified polystyrene. This material features fast set-up as well as easy colorability.Applications: API 545 is suggested for heavy parts with large cross section requiring high impact resistance. Housings, tote bins, shoe heels are some examples.Information provided by American Polymers, Inc.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Melt Flow 5.5 g/10 min
5.5 g/10 min
Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell L 47
47
ASTM D785
Tensile Strength, Ultimate 27.6 MPa
4000 psi
ASTM D638
Elongation at Break 58 %
58 %
ASTM D638
Tensile Modulus 1.93 GPa
280 ksi
ASTM D638
Flexural Modulus 2.10 GPa
305 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm

@Thickness 3.17 mm
1.90 ft-lb/in

@Thickness 0.125 in
injection molded sample; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
190 °F
Annealed; ASTM D648
Vicat Softening Point 98.9 °C
210 °F
ASTM D1525
Users viewing this material also viewed the following: