Dow Corning SE 4400 KIT

Category Polymer , Adhesive , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SE 4400 KIT.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Two-part, grey, heat cure, flowable, thermally conductive, UL V-0.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 2.15 g/cc

@Temperature 25.0 °C
2.15 g/cc

@Temperature 77.0 °F
Viscosity 76000 cP
76000 cP
dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
Tensile Strength, Ultimate 5.80 MPa
841 psi
Elongation at Break 90 %
90 %
Thermal Properties Metric English Comments
Thermal Conductivity 0.920 W/m-K
6.38 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Dielectric Strength >= 25.0 kV/mm
>= 635 kV/in
Processing Properties Metric English Comments
Cure Time 1020 min

@Temperature 150 °C
17.0 hour

@Temperature 302 °F
1020 min

@Temperature 22.0 °C
17.0 hour

@Temperature 71.6 °F
Shelf Life 7.00 Month
7.00 Month
Descriptive Properties Value Comments
Color grey
Flowable yes
Hydrophobic yes
Self Leveling yes
Water Resistant yes